Just a couple quick comments....
No need to go from 180 to 220. I usually go from 180 up to 320, but if you are spraying a 2k over the polyester, then just leave at 180 for the 2k. You will be sanding the 2k anyway.
Also, if you are spraying a metallic or pearl of any kind, be sure to sand your sealer for much better results. Do not spray a sealer just prior to the metallic, unless you sand it with 600 grit first.'67 Chevelle LS1 T56